FAQ Section: Common Questions Answered

What is anodizing and how does it work?
What are the key benefits of anodized aluminum?
- Enhanced Durability: Anodized finish is the second hardest substance known to man (exceeded only by diamond)
- Corrosion Resistance: Provides excellent protection against environmental factors
- UV Stability: Maintains color and performance even with prolonged sun exposure
- Aesthetic Appeal: Offers a wide range of color options and finishes
- Electrical Insulation: The oxide layer is non-conductive
- Easy Maintenance: Simple to clean and maintain its original appearance
Which aluminum alloys are best for anodizing?
- 6061-T6: Excellent all-around performer with good strength and corrosion resistance
- 7075-T6: High-strength alloy ideal for aerospace applications
- 2024-T3: Strong and fatigue-resistant, commonly used in aircraft structures
- 5052-H32: Superior corrosion resistance, perfect for marine environments

How long does the anodizing process take?
- Surface preparation: 30-60 minutes
- Anodizing process: 30-60 minutes
- Coloring (if required): 15-30 minutes
- Sealing: 20-30 minutes
- Quality inspection: 15-20 minutes
What color options are available?

Practical Guide: Step-by-Step Process

Step 1: Material Selection
Step 2: CNC Machining
- Program the CNC machine with precise dimensions
- Use proper cutting tools and speeds for aluminum
- Maintain tight tolerances (typically ±0.02mm)
- Ensure smooth surface finish (Ra 0.8-1.6μm)

Step 3: Surface Preparation
- Degreasing: Remove oils and contaminants using alkaline solutions
- Etching: Create uniform surface texture
- Desmutting: Remove smut and impurities
- Rinsing: Thoroughly clean parts between processes
Step 4: Anodizing Process
- Electrolyte Solution: Sulfuric acid (15-20%) at 18-22°C
- Current Application: 1-2 A/dm² at 12-20V
- Processing Time: 30-60 minutes for standard coating
- Film Thickness: 10-20μm for decorative, up to 100μm for hard anodizing

Step 5: Coloring (Optional)
- Organic Dyes: Wide color range, cost-effective
- Inorganic Coloring: More durable, limited color options
- Two-Step Process: Color independent of coating thickness
Step 6: Sealing
- Hot Water Sealing: 95-100°C for 30 minutes
- Cold Nickel Sealing: Room temperature, ideal for dyed parts
- Mid-Temperature Sealing: 80°C, environmentally friendly and efficient
Step 7: Quality Control
- Film Thickness Measurement: Using eddy current instruments
- Corrosion Testing: 5% NaCl salt spray test for 48 hours
- Adhesion Testing: Cross-hatch and tape tests
- Color Consistency: ΔE < 1.0 using spectrophotometer

Service Comparison: Anodizing vs. Other Surface Treatments
Cost Comparison

Performance Comparison

Key Differences
|
Feature
|
Anodizing
|
Powder Coating
|
Painting
|
|
Durability
|
Excellent (20+ years)
|
Good (15 years)
|
Fair (10 years)
|
|
Corrosion Resistance
|
Excellent
|
Good
|
Fair
|
|
UV Stability
|
Excellent
|
Good
|
Poor
|
|
Color Options
|
Limited
|
Extensive
|
Unlimited
|
|
Eco-Friendliness
|
Excellent
|
Good
|
Fair
|
|
Cost
|
Moderate
|
Low
|
Low
|
Conclusion

- Choose the right aluminum alloy for your specific application requirements
- Follow proper surface preparation and anodizing parameters
- Consider the total lifecycle cost rather than just initial investment
- Partner with experienced manufacturers for consistent quality results