Bubbles in injection molded parts are cavities formed by trapped gases, moisture vaporization, or vacuum voids due to uneven cooling and shrinkage, typically caused by material moisture, poor venting, process parameter issues, or mold design flaws.
Causes Bubbles in Injection Molded Parts

Types of Injection Molding Bubbles

Bubble Type
Appearance
Common Causes
Detection Method
Surface Bubbles
Small blisters on surface
Moisture, air entrapment
Visual inspection
Internal Voids
Hidden internal cavities
Poor venting, material issues
X-ray, sectioning
Vacuum Voids
Sink marks after cooling
Uneven cooling, shrinkage
Delayed appearance
Silver Streaks
Silver threads on surface
Volatile gases, decomposition
Visual inspection

Distribution of Bubble Causes

Bubble Causes Distribution

Troubleshooting Solutions Comparison

Troubleshooting Solutions Comparison

Professional Knowledge about Injection Molding Bubbles

Material-Related Causes

  • Moisture Content: Hygroscopic materials (PA, PC, PET) absorb moisture, which vaporizes during heating
  • Volatile Substances: Residual monomers, additives, or contaminants release gases at high temperatures
  • Material Degradation: Overheating causes polymer chain breakage and gas formation

Process Parameter Issues

  • Temperature Control: Excessive melt temperature leads to material decomposition
  • Injection Speed: Too fast causes turbulence and air entrapment
  • Pressure Settings: Insufficient injection/holding pressure fails to compact material
  • Screw Parameters: High speed/low back pressure allows air incorporation

Mold Design Factors

  • Venting System: Inadequate venting channels (0.02-0.05mm depth recommended)
  • Gate Design: Improper location or size causes flow imbalance
  • Runner System: Restrictive flow paths trap air
  • Cooling Uniformity: Uneven cooling creates temperature gradients

Environmental Factors

  • Humidity Control: High ambient humidity affects material moisture content
  • Contamination: Oil, dirt, or release agents introduce foreign substances
  • Storage Conditions: Improper material storage leads to moisture absorption

Frequently Asked Questions (FAQ)

Q1: How can I distinguish between different types of bubbles?

A: Surface bubbles appear immediately after molding, internal voids require sectioning/X-ray, vacuum voids appear after cooling, and silver streaks show as surface discoloration.

Q2: What is the most effective solution for moisture-related bubbles?

A: Proper material drying – use desiccant dryers with temperatures: PA (80-120°C), PC (120-130°C), PET (140-160°C) for 4-8 hours.

Q3: How should I design mold venting for bubble prevention?

A: Add vents at last fill locations, 0.02-0.05mm depth, 5-10mm width. Use porous steel inserts for complex areas.

Q4: What process parameters should I adjust first for bubbles?

A: Start with material drying, then reduce injection speed, increase holding pressure, and optimize melt temperature.

Q5: Can recycled materials cause more bubbles?

A: Yes, recycled materials often contain more moisture, contaminants, and volatile substances. Limit to 30% maximum.

Q6: How does mold temperature affect bubble formation?

A: Too low – rapid cooling traps gases; too high – material degradation. Maintain recommended mold temperatures.

Q7: What is the minimum drying requirement for hygroscopic materials?

A: Moisture content should be below 0.02% for most engineering plastics.

Q8: How can I prevent air entrapment during injection?

A: Use slower injection speeds, especially in thin sections, and implement multi-stage injection profiles.

Disclaimer
All experimental data presented in this paper are derived from controlled production environments and standardized test procedures. However, due to differences in equipment models, material batches, and on-site operating conditions, readers are advised to verify and adjust technical parameters according to their specific application scenarios before practical implementation.
The research results and technical insights shared herein are based on the author’s professional experience and experimental observations. The author and the affiliated institution shall not be liable for any direct, indirect, or consequential damages (including but not limited to equipment damage, product quality issues, or production losses) arising from the improper use of the information provided in this paper.
Please enable JavaScript in your browser to complete this form.
Please be sure to describe the specific customization requirements in detail. Otherwise, we will ignore the submitted content.

Recommended Reading